Principles of using pe butt welding machine

Dec 31, 2020

Adjust the distance between the jaws. When the control screw is at the left limit, the distance between the two welded parts is the difference between the length and the extrusion. When the joystick is at the appropriate limit, the distance between the clamps should be the length of the two welded parts and 2 ~ 3 mm, the position before welding.

Adjust the short-circuit limit switch so that the power supply will automatically cut off the power supply when the welding is completed (reaching the predetermined extrusion).

According to the shape of the welding workpiece, adjust the clamp, clamp the two clamps at the same level, and then clamp the welding part.

In order to prevent the welding parts from overheating instantaneously, an adjustment series should be added when testing welding, and an appropriate secondary voltage should be selected. In flash butt welding, a higher secondary voltage is used.

In order to avoid welding overheating, the cooling water valve must be opened before welding. In order to facilitate the inspection, a funnel is provided on the left side of the welder to directly observe the flow situation to check whether there is cooling water flow inside the welder.